Construction Materials Single Component PU Waterproof Coating (for Non
HomeHome > Products > Construction and Coatings > Construction Materials Single Component PU Waterproof Coating (for Non
Construction Materials Single Component PU Waterproof Coating (for Non

Construction Materials Single Component PU Waterproof Coating (for Non

Package Size20.00cm * 20.00cm * 30.00cm Package Gross Weight20.000kg Description Product is a moisture-cured waterproof
Basic Info.
Model NO. PU-1
Method Brush
Drying Method Moisture Cured
Property Waterproofing
Where to Use Roof
Customized Yes
Exposed Condition UV Resistant
Type Roofing and Waterproofing
Ceiling Tile Shape Liquid
Surface Treatment Roll Coated
Function Waterproof
Usage Outdoor, Indoor
After-sales Service 3-5years
Warranty 3-5years
Color Red, Grey, Black or Customized
Transport Package Pallet
Specification 20kg/pail
Trademark EONZEAL
Origin China
Production Capacity 19000 Tons Per Year
Packaging & Delivery
Package Size20.00cm * 20.00cm * 30.00cm Package Gross Weight20.000kg
Product Description

Description

Product is a moisture-cured waterproof coating, form a seamless film by absorbing moisture from the air; with high flexibility and elongation, strong ability to substrates deformation, waterproof life up to 15 years.


Feature & Benefit

1. Packed in one component and ready to use. It avoids the quality instability induced by the inappropriate compounding of two or three components.

2. The performance is stable. It possesses the property of aging-resistance, acid and alkali resistance, fatigue resistance as well as high and low temperature resistance.
3. Environmentally-friendly.

4. Good leveling property, simple construction. After coating, it will react with moisture in the air and cure, forming a compact, seamless, tough and high elastic waterproof film.

5. It can be compounded with high polymer membrane and self-adhesive modified bitumen waterproof membrane to form a compound waterproof system.

Main Application

1. Non-exposed roof

2. Underground

3. Indoor bathroom and kitchen

4. Non-potable water waterproof construction

Installation

Substrate Preparation

All Surfaces

The substrate needs to be strong and smooth, clean and dry. Fill the holes with cement mortar. The flaws such as honey comb should also be repaired.

The external and internal corner are made to be arc.

Internal corner: D≥ 50mm
External corner: D≥ 10mm.

Application Guidance

1. Leveling
Substrate should be smooth and firm.

2. Cleaning
No garbage, floating pulp on the substrate, keep it dry.

3. First coating
The first layer should be very thin, covering the substrate is enough, less than 0.5mm thickness.

4. Second & Third coatings
Apply the second layer provided the first layer is cured. Coating direction is vertical to the first one and then the third layer's direction is the same as the first one.

Supply

Coverage

Recommend dosage: 1.65 kg/sqm, 1mm thickness, total thickness no less than 1.5mm

Packaging

20kg/barrel

Shelf life

Do not store product exposed to weather and sun. When kept in a cool, dry and protect area, sealed pail have a 12-months shelf life.

Precaution

1. Second layer is the thickest one, the third one is very thin, just for leveling.

2. Interval time depends on the application site, but typically full drying time is about 20 hours.

3. Fiber reinforcing layer is necessary for inside corner internal corner, floor drain, pipe joints etc, the lap width should not be less than 100mm, extensive application after joints treatment.

4. Use PU out after opening, time within 30 minutes. Long-term storage will cause the forming of a thin film on the surface. Remove this when application. Does not affect the performance of product.


Construction Materials Single Component PU Waterproof Coating (for Non-Exposed Roof)

Red/Grey/Black Single Component PU Coating From China Factory
Single-component polyurethane waterproof coating

Technical Data Sheet
Implement Standard: GB/T19250-2013
NO. Item Standard Result
1 Features Uniform sticky liquid,
no gel and no lump
Pass
2 Solid content,% ≥ 85 90.4
3 Surface drying time, h≤ 12 8
4 Fully drying time, h≤ 24 20
5 Tensile strength, MPa≥ 2 2.97
6 Elongation at break,%≥ 500 542
7 Tear strength, N/mm≥ 15 26
8 Low temperature flexibility,ºC≤ -35 ºC no cracking Pass
9 Water tightness 0.3MPa 120min Watertight Pass